Comprasion of STEEL and FRP Rebars Physical Properties
Steel Rebar | FRP Rebar | |
Material | Steel | FRP |
Tensile Strenght, Mpa | 360 - 390 | 800 - 1300 |
Elastisite Modulü, Mpa | 200.000 | 55.000 |
Elongation at Fracture, % | 25 | 2 - 2,1 |
Linear Expansion Coefficient, 10-6/K | 13 - 15 | 9 - 12 |
Density, kg/dm³ | > 7 | 1,9 - 2,1 |
Length | 6 - 12 m | optionally |
Corrosion and Chemical Resistance | No | Yer |
Thermal Conductivity | Yes | No |
Dielectric | No | Yes |
Insensitive to Electromagnetic Fields | No | Yes |
Life Expectancy | 30 years | 100 years |
Comperasion according to Physical and wheight Conditions | Ø 6 | Ø 4 |
Ø 8 | Ø 6 | |
Ø 10 | Ø 7 | |
Ø 12 | Ø 8 | |
Ø 14 | Ø 10 | |
Ø 16 | Ø 12 | |
Ø 18 | Ø 14 | |
Ø 20 | Ø 18 |